Hard Aggregate Dry-Shake
SURFACE MODIFICATION WITH HARD AGGREGATE DRY-SHAKE
Hard aggregate dry-shake method is an alternative acc. to DIN 18560-3 and -4 to achieve a surface modification of a concrete floor. This surface modification serves to increase the wear resistance and the surface hardness, however, cannot be compared with a hard aggregate layer acc. to DIN 18560-7.
KORODUR dry-shake products are based on hard aggregates acc. to DIN 1100.
The dry-shake is carried out dry on the fresh screed or concrete surface – manually, with sprinkling cart or spreader.
HARD AGGREGATE DRY-SHAKE – THIS IS HOW IT WORKS

KORODUR GOES Green
Sustainability in the ecological sense has long been a matter of the heart for us, and we know that it will have a lasting impact on all aspects of construction. We are therefore expanding our range with new products whose manufacture involves significantly lower CO2 emissions. With the resource-saving NEODUR HE 3 green variant, we can already reduce CO2 emissions by up to 30 percent. We provide corresponding Environmental Product Declarations (EPDs) for builders, architects, planners, and construction companies.
NEODUR dry mortars
| Product | Quality | Group/DIN 1100 | Wear resistance |
|---|---|---|---|
| NEODUR HE 3 | CT-C70-F9-A6 | A | ≤ 5 cm³/50 cm² |
| NEODUR HE 3 green | CT-C70-F9-A6 | A | ≤ 5 cm³/50 cm² |
| KORODUR 0/4 | CT-C70-F10-A6 | A | ≤ 5 cm³/50 cm² |
| NEODUR HE 3 SVS 3 | CT-C70-F9-A3 | A | ≤ 3 cm³/50 cm² |
| NEODUR HE 3 SVS 1,5 | CT-C70-F9-A1,5 | KS | ≤ 1,5 cm³/50 cm² |
| NEODUR HE 3 SVS 1,5 extra | CT-C70-F9-A1,5 | ≤ 1,5 cm³/50 cm² | |
| NEODUR HE 3 metallic | CT-C80-F11-A3 | M | ≤ 3 cm³/50 cm² |
| NEODUR HE 2 | CT-C70-F9-A8 | ≤ 8 cm³/50 cm² |
NEODUR hard aggregate dry mortars are available also in colours see KORODUR colour chart.